10 TPH Φ2.5×40m Manganese Oxide Rotary Kiln Production Line in Chongqing, China

HONGKE CHINA Release Date: 2026-11-23 Views:

  • 10 TPH Φ2.5×40m Manganese Oxide Rotary Kiln Production Line in Chongqing, China

Project Overview

In this metallurgical engineering project, Henan Hongke Heavy Machinery Co., Ltd. designed, manufactured, and commissioned a high-efficiency 10 TPH Manganese Oxide Rotary Kiln production line for a leading manganese chemical and battery-grade material manufacturer in Chongqing, China.

Chongqing and its surrounding southwestern regions possess significant manganese ore resources, serving as a vital hub for Electrolytic Manganese Metal (EMM) and Electrolytic Manganese Dioxide (EMD) production. Converting raw pyrolusite (MnO2) into acid-soluble manganous oxide (MnO) requires precise reduction roasting under strictly controlled thermal and atmospheric conditions. Drawing on decades of heavy thermal equipment expertise, Henan Hongke Heavy Machinery Co., Ltd. delivered an automated, sealed Manganese Oxide Rotary Kiln production line built around our precision-engineered Φ2.5×40m Manganese Oxide Rotary Kiln.

Technical Highlights & Equipment Specifications

The core of this plant is the Φ2.5×40m Manganese Oxide Rotary Kiln, integrated with an enclosed quantitative feeding system, a sealed water-cooled discharge cooler, a waste-heat recovery unit, and a multi-stage dust purification system to form a turnkey Manganese Oxide Rotary Kiln production line.

ParameterSpecification / Value
Project LocationChongqing, China
Core EquipmentΦ2.5×40m Manganese Oxide Rotary Kiln
Production Line TypeComplete Reduction Roasting Manganese Oxide Rotary Kiln production line
Production Capacity10 Tons/Hour (240 Tons/Day / ~80,000 Tons/Year)
Raw MaterialPyrolusite Ore (MnO2, Grade: 25%–38%) + Reducing Agent (Anthracite / Coal)
Reduction Roasting Temperature750°C – 850°C (Controlled Reducing Atmosphere)
Kiln Inclination & Speed3.5% Inclination / Variable Frequency Drive (0.5 – 3.2 rpm)
Sealing & Atmosphere ControlDouble-Layer Flexible Graphite & Spring-Loaded Fish-Scale Seals
Cooling & Re-Oxidation PreventionSealed Indirect Water-Cooled Rotary Cooler (Discharge Temp less than 80°C)
Finished Product QualityManganese Reduction Rate ≥ 93%–95% / Acid Leaching Efficiency ≥ 94%

Key Challenges & Custom Engineering Solutions

1. Maintaining a Strict Reducing Atmosphere Without Air Leakage

  • Challenge: During manganese dioxide (MnO2) reduction roasting at 750°C–850°C, any ingress of external oxygen into the kiln cylinder causes re-oxidation of newly formed MnO back into acid-insoluble Mn3O4, drastically lowering downstream leaching yields.
  • Solution: Henan Hongke Heavy Machinery Co., Ltd. engineered the Φ2.5×40m Manganese Oxide Rotary Kiln with high-precision double-layer flexible graphite and spring-loaded fish-scale seals at both the feed hood and discharge hood. Combined with micro-positive pressure control inside the Manganese Oxide Rotary Kiln, oxygen leakage is virtually eliminated, ensuring a consistent reducing atmosphere throughout the 40-meter cylinder.

2. Preventing Re-Oxidation During High-Temperature Material Discharge

  • Challenge: Hot manganese oxide discharged at ~800°C will immediately re-oxidize if exposed to ambient air before cooling below 100°C.
  • Solution: Our engineers integrated an enclosed, indirect water-cooled rotary cooler directly coupled to the discharge hood of the Manganese Oxide Rotary Kiln production line. Roasted MnO calcine is cooled under an oxygen-isolated environment down to below 80°C before exiting to the leaching workshop, preserving a 94%+ manganese reduction rate.

3. Precise Temperature Control to Avoid Sintering & Ring Formation

  • Challenge: Manganese ores often contain iron, silica, and alumina impurities that can form low-melting-point silicates if local temperatures exceed 900°C, leading to kiln ring accretion and incomplete reduction.
  • Solution: The Manganese Oxide Rotary Kiln production line utilizes multi-point wireless thermocouple temperature monitoring along the kiln shell and a PLC-controlled variable-frequency drive. Operators maintain uniform bed temperatures between 780°C and 830°C, preventing ring buildup while cutting fuel consumption by 18%–22% through exhaust heat recycling.

Project Results & Customer Benefits

  • High Manganese Reduction & Leaching Yield: Calcined manganese oxide produced by the Φ2.5×40m Manganese Oxide Rotary Kiln consistently achieved a reduction rate of 93.5%–95.2%, boosting downstream sulfuric acid leaching efficiency and lowering acid consumption.
  • Stable 10 TPH Continuous Operation: Automated PLC control and heavy-duty mechanical construction enabled uninterrupted operation exceeding 330 days per year at a steady 10 tons per hour feed rate.
  • Clean, Compliant Industrial Emissions: Equipped with a cyclone pre-collector, waste-heat exchanger, and high-efficiency pulse baghouse dust collector, particulate emissions across the Manganese Oxide Rotary Kiln production line remain strictly below 10 mg/Nm³.

Turnkey Manganese Oxide Rotary Kiln Production Line Solutions by Henan Hongke

From manganese ore laboratory reduction testing and process flow engineering to heavy equipment fabrication, on-site installation, and operator training, Henan Hongke Heavy Machinery Co., Ltd. delivers turnkey EPC Manganese Oxide Rotary Kiln production lines for electrolytic manganese, manganese sulfate (battery-grade), and metallurgical enterprises worldwide. Whether you require a compact 5 TPH unit or a large-scale 10 TPH Φ2.5×40m Manganese Oxide Rotary Kiln, our engineering team ensures reliable performance and rapid ROI.

Planning a new manganese ore reduction roasting project? Contact Henan Hongke Heavy Machinery Co., Ltd. today to request a customized process flow diagram, equipment configuration list, and detailed technical proposal.
Tag: Manganese Oxide Rotary Kiln

Request Your Tailored Machinery & Plant Quotation

Connect with our engineering experts directly. Receive factory pricing and technical proposals within 12 hours.

TOP